Palm Oil Engineering Bulletin No.85 (Oct - Dec 2007) p27, 33-37
Welding technology for good milling practice: module 3 – welding equipments and welding defects
NARAYANAN, S.P

All welding machines are designed to step-down voltage – low voltage, high current and also taking safety factor into consideration. The secondary voltage, open circuit voltage (OCV) is in the range of 50 – 100 V with the current ratings varying from 5 A – 800 A.



Tags: , , ,

Author information:


Releated

Mongana basics: part 10-clarification of crude oil

Whatever the process used, crude oil must be refined. The complete refining of oil consists of the following operations: • separation of solid impurities that is impurities not soluble in oil, • separation of free water, • partial separation of dissolved moisture that is dehydration or drying, • de-gumming, • separation of free fatty acids […]